About this part
I printed this on a Prusa Mini+ with generic PETG using a 4mm nozzle by rotating the model to 315 degrees so it will fit diagonally. This was an absolute torture print for this printer.
Would recommend printing first layer at a much hotter than stock 240/260 temp for PETG or use glue stick or no fan if you print this. The point of failure is bed adhesion on the edges which get bridged together to the inner part on layer 3. If your first layer starts curling up, you're cooked.
at the 20% mark of the print is where you should watch for that. Once you get past the bridging on layer 3, you are in the clear.
I printed 15% infill, which barely saves you anything so feel free to print solid.
If you open this on PrusaSlicer or have a smaller bed and PrusaSlicer auto scales, just make sure your XYZ world scaling is 1 for proper fitting. For whatever reason it scales down for me even though you can rotate it to make it fit at 1-1-1 scaling.
XYZ
Position90901.5mm
Rotate (relative):000deg
Scale Factors111%
Size [world]184.257.043mm
Ensure that this is your scale, and rotate to fit.